INTERNATIONAL CLASSIFICATIONS

AWS/ASME A 5.11 ENiCrMo-4

EN/ISO 14172 ENi6276

DIN 1736: EL NiMo15Cr15W

NiCr15Mo15Fe6W4

FEATURES & APPLICATIONS
  • Excellent all position joining of corrosion resistant nickel base alloys.
  • Deposits are highly resistant to sulfuric acid environments.
  • Widely accepted throughout the chemical industry.
All Weld Metal Analysis (Typical Weight %)

Flux Color: Grey

CMnFePSSiCuCrMoVWNi
.02.94.9.04.02.19.4516.217.334.4Bal
Typical Mechanical Properties

Undiluted Weld Metal Maximum Value Up to:

Tensile Strength 110,000 PSI (760 MPa)

Yield Strength 65,000 PSI (460 MPa)

Elongation 34%

Welding Current & Instructions

Recommended Current: DC Reverse (+)

Diameter (mm)3/32 (2.5)1/8 (3.2)5/32 (4.0)
Minimum Amperage508090
11075110130

Welding Techniques: Use as low an amperage as possible, a short arc gap, and a stringer bead technique is preferred.

Welding Positions: Flat, vertical up, horizontal, overhead

Deposition Rates:

Diameter
(mm)
Length
(mm)
Weldmetal/
Electrode
Electrodes per lb (kg) of WeldmetalArc Time of Deposition min/lb (kg)Amperage Settings
3/32 (2.5)10″ (250).35 oz (10g)42 (92)45 (100)65
1/8 (3.2)14″ (350).76 oz (21g)23 (51)22 (49)90
5/32 (4.0)14″ (350)106 oz (31g)17 (37)20 (45)105
APPROXIMATE ELECTRODE PACKAGING & DIMENSIONS
3/32 (2.5)1/8 (3.2)5/32 (4.0)
Length (mm)10″ (250)14″ (350)14″ (350)
Electrodes / lb24139